IJSRP, Volume 11, Issue 9, September 2021 Edition [ISSN 2250-3153]
N. Wendri, W.G. Suharta
Abstract:
In this study, the wet-mixing method was used for synthesis (Ba0.95Ca0.05)TiO3 ceramic material, with Gd variations of 0.05, 0.10, 0.15, 0.20, 0.25. The study’s goal is to develop a piezoelectric material that has a high crystalline concentration and density. As source materials, BaCO3, TiO2, CaCO3, and Gd2O3 compounds were used. By weighing the raw material and dissolving it, the synthesis process can be completed.